TECHNYL STAR® A 205F NATURAL S

TECHNYL STAR
PA66
Thermoplastic-Polyamide-66

Solvay

Machanical Value Unit Condition Method
Izod Impact Strength(Iso), Notched 3.5 kJ/㎡ dry, 23°C ISO 180
Elongation At Break 110 % Conditioned, 23°C ISO 527-2
Charpy Impact Strength(Iso), Unnotched 10000000000 kJ/㎡ dry, 23°C ISO 179/1eU
Charpy Impact Strength(Iso), Notched 6.6 kJ/㎡ cond, 23°C ISO 179/1eA
Tensile Modulus 1300 MPa Conditioned, 23°C ISO 527-2/-1A
Tensile Strength At Break 79 MPa Conditioned, 23°C ISO 527-2/-1A
Charpy Impact Strength(Iso), Notched 3.4 kJ/㎡ dry, 23°C ISO 179/1eA
Tensile Modulus 3100 MPa dry, 23°C ISO 527-2/-1A
Charpy Impact Strength(Iso), Unnotched 10000000000 kJ/㎡ Conditioned, 23°C ISO 179/1eU
Elongation At Break 32 % dry, 23°C ISO 527-2
Tensile Strength At Break 80 MPa dry, 23°C ISO 527-2/-1A
Flexural Modulus 3070 MPa dry, 23°C ISO 178
Physical Value Unit Condition Method
Specific Gravity 1.14 dry ISO 1183/A
Water Absorption 1.5 % 23°C, 24hr ISO 62
Specific Gravity 1.15 dry ASTM D792
Water Absorption 2.8 % Equilibrium, 23°C/50%RH ISO 62
Thermal Value Unit Condition Method
Heat Deflection Temperature @1.82mpa 65 ˚C dry, 1.8MPa, Unannealed ISO 75-2/Af
Melting Temp 263 ˚C dry ISO 11357-3
Heat Deflection Temperature @0.46mpa 153 ˚C dry, 0.45MPa, Unannealed ISO 75-2/Bf
Electrical Value Unit Condition Method
Comparative Tracking Index(Cti) 600 V Dry, Solution A IEC 60112
Electric Strength 27 kV/mm dry, 2.0mm IEC 60243-1
Dielectric Constant 3.2 Conditioned IEC 60250
Electric Strength 26 kV/mm Conditioned, 2.0mm IEC 60243-1
Dielectric Constant 2.9 dry IEC 60250