HCPP BX3800
Impact PP
Thermoplastic-Polypropylene-Block_Hcpp
SK지오센트릭
| Machanical | Value | Unit | Condition | Method |
|---|---|---|---|---|
| Izod Impact Strength(Astm), Notched | 50 | J/m | -20°C | ASTM D256 |
| Tensile Strength At Yield | 32.36 | MPa | ASTM D638 | |
| Elongation At Break | % | ASTM D638 | ||
| Rockwell Hardness | 102 | R scale | ASTM D785 | |
| Flexural Modulus | 1863.26 | MPa | ASTM D790 | |
| Izod Impact Strength(Astm), Notched | 70 | J/m | 23°C | ASTM D256 |
| Physical | Value | Unit | Condition | Method |
|---|---|---|---|---|
| Melt Index | 30 | g/10min | ASTM D1238 |
| Thermal | Value | Unit | Condition | Method |
|---|---|---|---|---|
| Heat Deflection Temperature | 135 | ˚C | ASTM D648 | |
| Softening Temperature | 155 | ˚C | ASTM D1525 |
| Other | Value | Unit | Condition | Method |
|---|---|---|---|---|
| Thermal-Oxidative Stability | 350 | hr | ASTM D3012 | |
| Spiral Flow | 800 | mm | SK Method |